Customization: | Available |
---|---|
Feature: | Long Time Materials |
Shape: | Brick, Shape as Required |
Suppliers with verified business licenses
Audited by an independent third-party inspection agency
Material | Wt% Tungsten Content |
Wt% Copper Content |
g/ Density at 20ºC |
W/M.K Thermal conductivity at 25ºC |
(10-6/k) Coefficient of thermal expansion at 20ºC |
W90Cu10 | 901 | Balance | 17.0 | 180-190 | 6.5 |
W85Cu15 | 851 | Balance | 16.4 | 190-200 | 7.0 |
W80Cu20 | 801 | Balance | 15.6 | 200-210 | 8.3 |
W75Cu25 | 751 | Balance | 14.9 | 220-230 | 9.0 |
W50Cu50 | 501 | Balance | 12.2 | 310-340 | 12.5 |